TP10
Toyolac Parrel / General purpose |
| Properties |
Test
Method |
Test
Condition |
Units |
TP10 |
| Tensile Strength |
ASTM-D638 |
23 C/
50%RH |
MPa
kg/cm2
|
46
470 |
Tensile Elongation
at Break |
23 C/
50%RH |
% |
>10 |
| Flexural Strength |
ASTM-D790 |
23 C/
50%RH |
MPa
kg/cm2
|
73
740 |
| Flexural Modulus |
23 C/
50%RH |
MPa
kg/cm2
|
2,160
22,000 |
| Izod Impact Strength |
ASTM-D256 |
23 C
12.7mm
V-notched |
J/m
kg cm/cm
|
186
19 |
-30 C
12.7mm
V-notched |
39
4 |
23 C
3.2mm
V-notched |
69
7 |
Distortion Temperature
Under Load |
ASTM-D648 |
6.4mm
1.82MPa |
C |
86 |
| Rockwell Hardness |
ASTM-D785 |
23 C/
50%RH |
R-SCALE |
109 |
| Melt Flow Rate |
ISO-1133 |
220 C/98N |
g/10min |
27 |
| Specific Gravity |
ASTM-D792 |
23 C/
50%RH |
- |
1.05 |
| Specific Surface Resistivity |
ASTM-D257 |
After
injection molding
23 C/50%RH
24hr |
 |
1 1011 |
| Charged Voltage |
*TORAY |
V |
660 |
Charged Voltage
Attenuation Half-Life |
*TORAY |
Sec. |
0.4 |
| Light Transmission |
JIS
K7105 |
23 C/
50%RH
3mm |
% |
- |
| Ball Pressure
Temperature |
C |
95 |
| Flammability |
UL94
File No.E41797 |
HB equivalent |
| Mold Shrinkage |
% |
0.5-0.7 |
|
|
Note ; These values are typical data for this product
under specific test conditions and not intended for use
as limiting specifications. *This grade doesn't contain
specific bromine flame retardant {PBB, PBBE(O), PBDE(O),
PBDPE(O)}. |
|
|
|
|